TiSiN nanocomposite coatings by chemical vapor deposition in a fluidized bed reactor at atmospheric pressure (AP/FBR-CVD)

J. Perez-Mariano, K. H. Lau, A. Sanjurjo, J. Caro, D. Casellas, C. Colominas

Producción científica: Artículo en revista indizadaArtículorevisión exhaustiva

37 Citas (Scopus)

Resumen

TiSiN nanocomposite coatings were deposited on stainless steel by chemical vapor deposition in a fluidized bed reactor at atmospheric pressure (AP/FBR-CVD) by reaction of TiCl4 and SiCl4 with NH3 at 850 °C. Coatings were characterized by means of GD-OES, XPS and XRD. TiSiN coatings with a Si content of 9 at.% showed a hardness of 28 GPa (the hardness of TiN and SiNx coatings was around 21 GPa) and a lower oxidation rate under dry air at 600 °C. Our results show for the first time that AP/FBR-CVD can be tuned for the deposition of nanocomposite ceramic coatings.

Idioma originalInglés
Páginas (desde-hasta)2217-2225
Número de páginas9
PublicaciónSurface and Coatings Technology
Volumen201
N.º6
DOI
EstadoPublicada - 4 dic 2006

Huella

Profundice en los temas de investigación de 'TiSiN nanocomposite coatings by chemical vapor deposition in a fluidized bed reactor at atmospheric pressure (AP/FBR-CVD)'. En conjunto forman una huella única.

Citar esto